Aluminum board process-A

the production of aluminum pcb specification
1. Preface: with the development and progress of electronic technology, electronic products to the light, thin, small, personalization, high reliability, muti_function change has become an inevitable trend.And out of aluminum plate conform to this trend, the product with excellent heat resistance, machinability, dimensional stability and electrical performance in hybrid integrated circuit, automobiles, office automation, high-power electrical equipment, power equipment, and other fields has been widely applied in recent years.Aluminium base copper clad by Japanese sanyo company first invented in 1969, our country began in 1988, development and production of Edna, developed and mass production began in 2000 in order to adapt to the mass production, mass production, artificial this production specification.     
2. Scope: this production specifications for the production of aluminium base copper clad introduces the whole process and specification, to ensure that the board in our production smoothly.    
3. Process: cutting and drilling→ dry film optical imaging→check board→etching→ corrosion inspection→solder mask→character →green inspection→ HASL→aluminum surface treatment→impact→final inspection→packaging→shipment   
4. Note:    
4.1 aluminum sheet is expensive, should pay special attention to the standardization of operation in the process of production, put an end to scrap phenomenon caused by the non-standard operations.   
4.2 each working procedure is operated operators must take put down gently, in order to avoid the plate and aluminum surface clean.
4.3 operators, each process should try to avoid hand contact with aluminum plate, the effective area after spray tin and process the board shall hold the edge, only when it is strictly prohibited to finger directly touch the board inside.
4.4 aluminum board belongs to the special board, should cause district attaches great importance to each process and its production supervisor, foreman, personal quality, guarantee the smooth plate in the process of production.    
5. The special production process flow and parameters:   
5.1 material cutting
5.1.1 strengthen incoming inspection (must use aluminum sheet metal surface has a protective film).
5.1.2 without baking plate after cutting.
5.1.3 light to take light put, pay attention to the protection of the aluminum surface (protective film).
 5.2 drilling
5.2.1 drilling parameters and FR - 4 plate drilling parameters are the same.    
5.2.2 aperture tolerance yan, 4 oz base Cu attention to control the generation of the beatles feng.
5.2.3 requires copper on the hole.
5.3 the dry film
5.3.1 incoming inspection: before grinding plate must be inspection on aluminum surface protective film, if there is any breakage, must be fastened with welan again after pretreatment.     
5.3.2 grinding plate: only on copper surface for processing.
5.3.3 the paster: copper, aluminum surface shall be sticker.
Control grinding plate and the lamination time interval is less than 1 minute, ensure the paster temperature stability.
5.3.4 clappers: pay attention to the clappers precision.
5.3.5 exposure, exposure ruler: 7 ~ 9 have glue.
5.3.6 development: stress: 20 ~ 35 psi speed: 2.0 ~ 2.6 m/min, the operator must be careful operation, avoid the protective film and aluminum chafed below.
5.3 the dry film
5.3.1 incoming inspection: before grinding plate must be inspection on aluminum surface protective film, if there is any breakage, must be fastened with welan again after pretreatment.

2015年3月9日星期一

Electronic Lead Free Assembly

Transitioning to lead-free assembly electronics requires not only product reliability, but also the ability for an optimized assembly process. Additionally, material selection, component changes, and handling potential testing failures are integral to a successful transition.

Choosing Materials
Surface finish is one of the key material choices impacting the entire assembly electronics process. The assembly process itself, plus the complexity of the board and its use environment, all make an impact on this decision. Typical options include lead-free HASL or ENIG, OSP, ImAg, and ImSN, with new innovations becoming market-ready all the time. Different laminates are often under-specified due to underestimating their quality during the assembly process. Alternatively, laminates may be over-specified, which commands a higher cost.

Solder alloys are another important decision: wave solder, surface mount, and solder for BGA balls all have to be considered. Typically, SAC305 is the surface-mount alloy of choice, and it performs acceptably under most circumstances. Depending on the complexity required for your wave solder alloys, the most cost effective solution is SnCU, especially if you have thin boards with low-aspect holes that need to be filled. SnAgCuNi is preferable for more challenging holes, although this may depend on the surface finish and choice of flux as well. For board flexing capabilities, or withstanding shock events, a variety of lower modulus alloys like SAC105 are becoming more prevalent.

Component Qualifications and Testing
Early adopters of lead-free assembly electronics discovered frequent occurrences of melted plastic components on wave solder connectors. This lead to a switch away from nylon 66 toward the more appropriate nylon 46, or sometimes LCP. These meet the requirements of moisture and temperature sensitivity, a must-have in surface-mount LF components.

Other components that need to withstand heat damage may be more difficult to detect, which makes preventing that damage a greater challenge. Electrolytes within electrolytic capacitors may boil if time limits and safety temperatures are exceeded, yet these limits are not always outlined in sufficient detail.

Common specs may offer some suggestions, yet without the necessary variables to predict possible behavior. Component engineers end up guessing at preheat durations and total peak heat, while attempts are made with lead-free alloys to properly fill holes under various conditions.

Testing the strain capability of separate components following lead-free assembly is another blind spot. For example, it’s commonly known that SAC alloys have a reduced tolerance for strain, yet their assembly manufacturing people rarely offer specific limits for these devices. If suppliers could record results of four-point bend testing for their components in order to determine an objective maximum strain capability, the user could know if problems are more likely to arise during component stuffing, performing ICT, or attaching their boards to the chassis.

Reworking
All too often, lead-free reworks are overlooked in favor or meeting tight manufacturing schedules. However, records indicate that reworking is one of the greatest challenges involved with making the transition to lead-free assembly. A Lead-free assembly electronic has a more difficult window lying between the cold solder on one end and heat damage at the other.

Reworking can bring operator-to-operator benefits to the mix, optimizing equipment process that was probably originally designed for Sn-Pb rework. Every critical component requires a strict rework process which must be rigidly adhered to. Extensive failure analysis has to be undertaken before a determination regarding appropriate rework procedure can be made. Damage to the PCBA manufacturer, the component itself, or any neighboring components must be prevented. New rework equipment may be necessary, as well as the employment of new shielding techniques.

Implement Auditing
Despite the growing experience with assemblage of lead-free PCBs, high quality is not always maintained after high-volume production begins. A comprehensive audit plan should be in place to address with the supplier in order to ensure accountability.  Making the change to lead-free assembly electronics provides an excellent opportunity to review your supplier’s typical process, and make any necessary adjustments for optimum quality control.

2015年3月3日星期二

System Level Design for My Bluetooth LED Lamp

System Level Design for My Bluetooth LED Lamp, yes I make Visio drawings for fun.
You may not know specifics like what supply voltages you will need or what connections need to be made, but you will be able to consider how each component will rely on the others and what additional components they will add to your design.
This is also a good time to consider the aesthetic aspect of your design. Are you trying to fit a certain form factor? Do you need to consider ergonomics (for example if you are designing a game controller)? Will you be able to pick up your design a year from now and understand exactly how it works? These are the types of details Aluminum pcb, while seemingly insignificant, can be the difference between a good design and a great design.
I know all this talk of visualization may sound cheesy and like it won’t really get you anywhere, but I assure you it is worthwhile. If you don’t want to believe me, consider this quote from Nikola Tesla’s autobiography where he describes his creative process:
My method is different. I do not rush into actual work. When I get an idea I start at once building it up in my imagination. I change the construction, make improvements and operate the device in my mind. It is absolutely immaterial to me whether I run my turbine in thought or test it in my shop. I even note if it is out of balance. There is no difference whatever, the results are the same.
Of course the vast majority of us aren’t at the level of crazed genius that is Tesla, but the idea behind this method is all the same. By visualizing your design beforehand you save time, money, and frustration.
Following will be continued in next chapter.
Shirley Xia
Wonderful PCB
T +86-755-86229518-636
e  wonderful25@wonderfulpcb.com |
w  www.wonderfulpcb.com  | Skype:wonderful-pcb02